• 中国科技论文统计源期刊
  • 中文核心期刊
  • 中国科技核心期刊
  • 中国机械工程学会无损检测分会会刊
高级检索

基于数字探测器阵列技术的带包覆层管道腐蚀检测

刘怿欢, 陈乐, 李卫星, 赵聪

刘怿欢, 陈乐, 李卫星, 赵聪. 基于数字探测器阵列技术的带包覆层管道腐蚀检测[J]. 无损检测, 2020, 42(2): 35-37. DOI: 10.11973/wsjc202002008
引用本文: 刘怿欢, 陈乐, 李卫星, 赵聪. 基于数字探测器阵列技术的带包覆层管道腐蚀检测[J]. 无损检测, 2020, 42(2): 35-37. DOI: 10.11973/wsjc202002008
LIU Yihuan, CHEN Le, LI Weixing, ZHAO Cong. Corrosion measurement of pipeline with cladding layer based on DDA[J]. Nondestructive Testing, 2020, 42(2): 35-37. DOI: 10.11973/wsjc202002008
Citation: LIU Yihuan, CHEN Le, LI Weixing, ZHAO Cong. Corrosion measurement of pipeline with cladding layer based on DDA[J]. Nondestructive Testing, 2020, 42(2): 35-37. DOI: 10.11973/wsjc202002008

基于数字探测器阵列技术的带包覆层管道腐蚀检测

详细信息
    作者简介:

    刘怿欢(1983-),男,高级工程师,主要从事特种设备无损检测工作

    通讯作者:

    刘怿欢, E-mail:liuyihuan@hotmail.com

  • 中图分类号: TG115.28

Corrosion measurement of pipeline with cladding layer based on DDA

  • 摘要: 压力管道在长期运行过程中,容易受内外介质的化学或电化学腐蚀而出现壁厚减薄的现象,壁厚减薄严重时会影响生产安全。通常,对压力管道腐蚀进行常规检测时需拆除包覆层,耗费大量的人力物力,应用可行性较差。针对该问题,提出基于数字探测器阵列(DDA)检测技术的带包覆层管道腐蚀的检测方法,试验分析了该方法的检测精度,并提出改进措施与进一步的研究方向。
    Abstract: During the long-term operation of the pressure pipeline, its wall is easy to be thinned by the chemical corrosion with the internal and external media, which will affect the industrial production. In the conventional corrosion measurement, the cladding layer needs to be removed, thereby causing a certain waste of human and material resources. Aiming at this phenomenon, this paper proposes a method for measuring corrosion of pipelines without dismantling the cladding layer based on DDA detection technology. The measurement accuracy of this method was analyzed by a series of tests, and then the improvement measures and further research directions were proposed.
  • [1] 巨西民,蒋中印,兰川,等.埋弧焊钢管焊缝DR检测机理及应用[J].无损检测,2014,36(10):29-31.
    [2] 刘彬.锅炉水冷壁管腐蚀检测[J].无损探伤,2012,36(5):47-48.
计量
  • 文章访问数:  7
  • HTML全文浏览量:  4
  • PDF下载量:  4
  • 被引次数: 0
出版历程
  • 收稿日期:  2019-06-30
  • 刊出日期:  2020-02-09

目录

    /

    返回文章
    返回